Volume 40 Issue 3
Sep.  2026
Turn off MathJax
Article Contents
LIU Guiping, LI Xia, JIA Wenqi. Influence analysis of temperature and humidity change on rail corrugation in small radius curves[J]. Journal of Shanghai University of Engineering Science, 2026, 40(3): 255-261. doi: 10.12299/jsues.25-0002
Citation: LIU Guiping, LI Xia, JIA Wenqi. Influence analysis of temperature and humidity change on rail corrugation in small radius curves[J]. Journal of Shanghai University of Engineering Science, 2026, 40(3): 255-261. doi: 10.12299/jsues.25-0002

Influence analysis of temperature and humidity change on rail corrugation in small radius curves

doi: 10.12299/jsues.25-0002
  • Received Date: 2025-01-02
  • Publish Date: 2026-09-30
  • To investigate the influence of environmental temperature and humidity changes on rail corrugation in small-radius curve sections and to formulate a more scientific control strategy for rail corrugation. A vehicle-track dynamics model and a three-dimensional wheel-rail finite element model were established. Based on the friction self-excited vibration theory, the effects of temperature and humidity were incorporated into the finite element model for complex eigenvalue calculation. By adjusting the friction coefficient and fastener stiffness in the model, the occurrence trend and influence law of rail corrugation under temperature and humidity changes were studied. The results show that when the curve radius is 400 m and the running speed is 60 km/h, the main frequency at which the wheel-rail system is most likely to occur friction self-excited vibration is 470.88 Hz, which causes short-wave corrugation of 30~40 mm on the low-rail surface. The relative humidity is negatively correlated with the absolute value of the equivalent damping ratio of the wheel-rail system. In addition, low-frequency vibration is sensitive to changes in the service environment temperature. In particular, under low-temperature conditions, the stiffness of the fastener system increases, exacerbating the generation of rail corrugation. Low temperature and low relative humidity are more likely to induce rail corrugation; therefore, attention should be paid to the prevention and control of rail corrugation in such environments.
  • loading
  • [1]
    Zhu Y, Lyu Y, Olofsson U. Mapping the friction between railway wheels and rails focusing on environmental conditions[J] . Wear, 2015, 324-325: 122 − 128.
    [2]
    Shi L B, Ma L, Guo J, et al. Influence of low temperature environment on the adhesion characteristics of wheel-rail contact[J] . Tribology International, 2018, 127: 59 − 68. doi: 10.1016/j.triboint.2018.05.037
    [3]
    肖乾, 方姣, 杨逸航, 等. 不同温湿度对高速列车车轮磨耗的影响分析[J] . 机械工程学报, 2018, 54(4): 14 − 21. doi: 10.3901/JME.2018.04.014
    [4]
    韦凯, 张攀, 豆银玲, 等. 高速铁路无砟轨道扣件系统弹性垫板力学性能的温变试验[J] . 铁道学报, 2016, 38(7): 98 − 104. doi: 10.3969/j.issn.1001-8360.2016.07.014
    [5]
    成功, 陈宗平, 肖新标, 等. 低温条件对板式高速铁路轮轨滚动噪声的影响研究[J] . 机械工程学报, 2023, 59(10): 187 − 196. doi: 10.3901/JME.2023.10.187
    [6]
    Zhai Z H, Zhu S Y, Yuan X C, et al. Nonlinear effects of a new mesh-type rail pad on the coupled vehicle-slab track dynamics system under extremely cold environment[J] . Proceedings of the Institution of Mechanical Engineers, Part F: Journal of Rail and Rapid Transit, 2023, 237(3): 285 − 296. doi: 10.1177/09544097221107472
    [7]
    Zhou L, Wang W J, Hu Y, et al. Study on the wear and damage behaviors of hypereutectoid rail steel in low temperature environment[J] . Wear, 2020, 456/457: 203365.
    [8]
    马超智. 高速铁路无砟轨道轮轨周期性磨耗形成机理及控制研究[D] . 北京: 北京交通大学, 2022.
    [9]
    文永蓬, 董昊亮, 徐祖翰, 等. 考虑温湿变的地铁曲线啸叫噪声形成机理分析[J] . 机械工程学报, 2025, 61(6): 217 − 227. doi: 10.3901/JME.2025.06.217
    [10]
    叶榕伟, 王欣纪, 邹港, 等. 不同温度和湿度下激光熔覆304L不锈钢局部修复车轮的摩擦磨损性能[J] . 机械工程材料, 2025, 49(1): 89 − 96. doi: 10.11973/jxgccl230599
    [11]
    石玉. 地铁A、B型车动力学性能对比分析[D] . 大连: 大连交通大学, 2017.
    [12]
    刘春阳. 一系悬挂和扣件参数对钢轨波磨影响的仿真分析[D] . 成都: 西南交通大学, 2018.
    [13]
    Lyu Y Z, Bergseth E, Olofsson U. Open system tribology and influence of weather condition[J] . Scientific Reports, 2016, 6(1): 32455. doi: 10.1038/srep32455
    [14]
    Li W, Wang H Y, Wen Z F, et al. An investigation into the mechanism of metro rail corrugation using experimental and theoretical methods[J] . Proceedings of the Institution of Mechanical Engineers, Part F: Journal of Rail and Rapid Transit, 2016, 230(4): 1025 − 1039. doi: 10.1177/0954409715596182
    [15]
    崔晓璐. 地铁线路钢轨波磨现象发生机理研究[D] . 成都: 西南交通大学, 2017.
    [16]
    Olofsson U , Sundvall K. Influence of leaf, humidity and applied lubrication on friction in the wheel-rail contact: Pin-on-disc experiments[J] . Proceedings of the Institution of Mechanical Engineers Part F: Journal of Rail and Rapid Transit, 2004, 218(3): 235 − 242.
    [17]
    陈宗平, 成功, 刘清源, 等. 高速铁路扣件动刚度频变和温变特性研究[J] . 振动、测试与诊断, 2022, 42(3): 495 − 502,616-617. doi: 10.16450/j.cnki.issn.1004-6801.2022.03.012
    [18]
    韦凯, 周昌盛, 王平, 等. 扣件胶垫刚度的温变性对轮轨耦合随机频响特征的影响[J] . 铁道学报, 2016, 38(1): 111 − 116. doi: 10.3969/j.issn.1001-8360.2016.01.018
    [19]
    Chen G X, Zhou Z R, Ouyang H, et al. A finite element study on rail corrugation based on saturated creep force-induced self-excited vibration of a wheelset–track system[J] . Journal of Sound and Vibration, 2010, 329(22): 4643 − 4655. doi: 10.1016/j.jsv.2010.05.011
    [20]
    Grassie S L. A practical methodology to prioritise reprofiling sites for corrugation removal[J] . Proceedings of the Institution of Mechanical Engineers, Part F: Journal of Rail and Rapid Transit, 2020, 234(4): 362 − 369. doi: 10.1177/0954409719853071
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Figures(6)

    Article Metrics

    Article views (45) PDF downloads(12) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return